Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPP 25-0216 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm |
16.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Oxford Polymers PC 714-FR Series PC, Flame retardant Product Description: Amorphous, Polycarbonate injection molding grade, flame retardant Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and UV stabilizersSpecial.. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Hylon® N1200STHL BK Nylon 6/6 Available in North America Additive: Heat Stabilizer and Lubricant Features: Lubricated, Good Toughness and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackInformation provided by Ravago. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm |
16.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-10R-CL(15) 15 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm |
16.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-10R-CL(V) 10 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 8.54 J/cm @Temperature -30.0 °C |
16.0 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
DuPont Bexloy® AXW504BK Modified Ionomer Resin
(discontinued **) A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B.. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Hylon® N1000STHLUV2 HF Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat Stabilized and High FlowRoHS CompliantAuto Specifications: GM GMP.PA66.074.. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | 73°F; ASTM D256 |
M. Holland Company PC402R Polycarbonate High clarityHigh heat resistanceHigh impact resistanceGood mold releaseApplications: AppliancesContainersTable products |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Global PC-1415-GY-802-R General Purpose Gray Polycarbonate Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Global PC-1603 Standard Grade Polycarbonate Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 8.54 J/cm @Temperature 22.8 °C |
16.0 ft-lb/in @Temperature 73.0 °F |
0.125"; ASTM D256 |
LTL Color Compounds ColorRxâ„¢ PC-1005ARX Biocompatible Polycarbonate A biocompatible, 10 melt grade of Polycarbonate for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided by LTL Col.. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm |
16.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6 IM HS L BK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUL File Number: E157318Processing Method: In.. |
|||
Izod Impact, Notched | 8.54 J/cm @Thickness 3.17 mm |
16.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6 IM L Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | >= 8.54 J/cm @Thickness 3.17 mm |
>= 16.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 L UV (Conditioned) Availability: North AmericaForms: PelletsAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 200 15 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 2071 15 Polycarbonate, Sterilization Grade CALIBRE® 2071 resins are designed for those applications which use steam or ethylene oxide for sterilization while providing enhanced mold release characteristics. This material has excellent ret.. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | 0.125 in; 10 mil notch; ASTM D256 |
Styron CALIBREâ„¢ 301-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 603 5 Polycarbonate, Branched CALIBRE® 603 is a branched polycarbonate resin and is equipped with a mold release and a UV stabilization package. CALIBRE 603 resins exhibit an excellent property balance of high clarity, high m.. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Styron EMERGEâ„¢ 4310-15 Polycarbonate EMERGEâ„¢ PC 4310-15 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® 627L Nylon 6/6 (DAM) Polifil® NYLON 6/6 combines good abrasion and chemical resistance.Applications: ValvesBearingsBearing casesStandard processing techniques are applicable. Information provided by The Plastics Group... |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Entec Hylex® P1307L1 HB Polycarbonate UV Stabilized, Low Flow, Mold Release, Water ClearInformation provided by Entec. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
Applied Composites 8092 Polyester SMC Industry Application: ConstructionProduct Application: Building ProductsDistinct Features: Pigmentable, High Molding Efficiency, Low Thermal ExpansionInformation provided by Applied Composites Corpo.. |
|||
Izod Impact, Notched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D256 |
PlastxWorld CEVIAN® A1500 PA/ABS Alloy, Conditioned Property data is for samples at equilibrium moisture (2.0%)Information provided by PlastxWorld Inc. |