Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 450 °C | 842 °F | Continuous |
Mykroy/Mycalex MM 451 Molding Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwid.. |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | |
Resinlab® RC8040 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | |
GrafTech GRAFOIL® GHC Standard Internal Combustion Laminate GRAFOIL® Grade GHC is a laminate made from Grade GTC flexible graphite. Laminate Construction: GRAFOIL® Grade GTC ? Micro-thin, phenolic-based adhesive ? GRAFOIL® Grade GTC |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | |
GrafTech GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material GRAFOIL® GTA premium flexible graphite is a non-inhibited grade developed for use in nuclear or semiconductor applications. It is certified to meet the most rigorous purity specifications of the .. |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | |
GrafTech GRAFOIL® GTC Standard Internal Combustion Graphite, Single Layer Material GRAFOIL® GTC flexible graphite sheet is a gasketing material containing no binders or fillers, which will seal a wide variety of liquids and gases over an extremely large temperature range. GTC c.. |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | Short Term; ASTM 5026 |
Specialty Coating Systems Parylene HT® Poly (P-Xylylene) Coating Parylene HT is a polymer of para-xylylene with the alpha hydrogen atoms of the N dimer replaced with fluorine. This variant of Parylene is useful in high temperature applications (short term up to 4.. |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | Long Term, depends on temperature gradient |
Schott BOROFLOAT® Borosilicate Float Glass This is a highly chemically resistant borosilicate glass with a low thermal expansion. BOROFLOAT® replaced TEMPAX®, a drawn flat borosilicate glass for Schott. The high quality resulting fro.. |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | |
Eifeler Coatings Technology TiN/TiC CVD Coating The titanium nitride / titanium carbide combination layer is a standard layer well-proven over a long time. It indicates the following properties: Very high hardness; Very good adhesion; Suffic.. |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | |
Alliance A-2 Alnico Magnetic Material |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | |
Alliance A-3 Alnico Magnetic Material |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | |
Alliance A-5S Alnico Magnetic Material |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | |
Alliance A-8S Alnico Magnetic Material |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | |
Alliance A-6S Alnico Magnetic Material |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | |
Alliance A-2S Alnico Magnetic Material |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | |
Resinlab® RC8020 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | |
Resinlab® RC8080 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | |
Resinlab® TL5072 Anaerobic Threadlocking Compound The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a .. |
|||
Maximum Service Temperature, Air | 450 °C | 842 °F | Oxidizing atmosphere |
Sinotek Materials Packing Expanded Graphite Braided Graphite braided packing, made of expanded graphite yarn braids, is resistant to heat, chemicals, and tight sealing. It is widely used in the steam valves of power plants, or as static sealing in pl.. |