Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Permeability 0.220 g mil/ (m2 day)

@Temperature 38.0 °C
0.0142 g mil/ (100 in2 day)

@Temperature 100 °F
100% RH; ASTM F1249
Specialty Coating Systems Parylene HT® Poly (P-Xylylene) Coating
Parylene HT is a polymer of para-xylylene with the alpha hydrogen atoms of the N dimer replaced with fluorine. This variant of Parylene is useful in high temperature applications (short term up to 4..