Material Notes:
Parylene D is a polymer of para-xylylene modified by the substitution of chlorine atoms for two of the aromatic hydrogen atoms. Parylene D is similar in properties to Parylene C with the added ability to withstand slightly higher use temperatures.SCS Parylene conformal coatings are ultra-thin, pinhole-free polymer coatings that provide a number of high-value surface treatment properties such as excellent moisture, chemical and dielectric barrier properties, thermal and UV stability, and dry-film lubricity. Parylene coatings are used in a number of applications throughout the medical device, electronics, automotive, military and aerospace industries.Information provided by Specialty Coating Systems (SCS) .
Physical Properties Metric English Comments
Water Vapor Permeability 0.0900 g mil/ (m2 day)

@Temperature 37.0 °C
0.00581 g mil/ (100 in2 day)

@Temperature 98.6 °F
90% RH; ASTM E96
Density 1.418 g/cc
0.05123 lb/in³
ASTM D1505
Water Absorption <= 0.10 %

@Time 86400 sec
<= 0.10 %

@Time 24.0 hour
ASTM D570
Oxygen Transmission 12.6 cc-mm/m²-24hr-atm

@Temperature 25.0 °C
32.0 cc-mil/100 in²-24hr-atm

@Temperature 77.0 °F
ASTM D1434
Nitrogen Transmission 1.80 cc-mm/m²-24hr-atm

@Temperature 25.0 °C
4.57 cc-mil/100 in²-24hr-atm

@Temperature 77.0 °F
ASTM D1434
Carbon Dioxide Transmission 5.10 cc-mm/m²-24hr-atm

@Temperature 25.0 °C
13.0 cc-mil/100 in²-24hr-atm

@Temperature 77.0 °F
ASTM D1434
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Yield 62.1 MPa
9000 psi
ASTM D882
Elongation at Break <= 200 %
<= 200 %
ASTM D882
Elongation at Yield 3.0 %
3.0 %
ASTM D882
Modulus of Elasticity 2.62 GPa
380 ksi
Secant; ASTM D882
Coefficient of Friction, Dynamic 0.31
0.31
ASTM D1894
Coefficient of Friction, Static 0.33
0.33
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear 38.0 µm/m-°C
21.1 µin/in-°F
via TMA
Melting Point 380 °C
716 °F
via DSC
Maximum Service Temperature, Air 100 °C
212 °F
Continuous
120 °C
248 °F
Short Term
Softening Point 125 °C
257 °F
T5 Point; modulus = 690 MPa (100,000 psi)
240 °C
464 °F
T4 point; modulus = 70 MPa (10,000 psi)
Optical Properties Metric English Comments
Refractive Index 1.669
1.669
n<sub>D</sub>; Abbe Refractometer
Transmission, Visible 87 %

@Wavelength 400 nm
87 %

@Wavelength 400 nm
UV Transmittance <= 1.0 %

@Wavelength 290 nm
<= 1.0 %

@Wavelength 290 nm
cutoff
30 %

@Wavelength 300 nm
30 %

@Wavelength 300 nm
80 %

@Wavelength 350 nm
80 %

@Wavelength 350 nm
Electrical Properties Metric English Comments
Volume Resistivity 1.20e+17 ohm-cm
1.20e+17 ohm-cm
50% RH; ASTM D257
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
50% RH; ASTM D257
Dielectric Constant 2.8

@Frequency 1.00e+6 Hz
2.8

@Frequency 1.00e+6 Hz
ASTM D150
2.82

@Frequency 1000 Hz
2.82

@Frequency 1000 Hz
ASTM D150
2.84

@Frequency 60.0 Hz
2.84

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 217 kV/mm
5500 kV/in
ASTM D149
Dissipation Factor 0.0020

@Frequency 1.00e+6 Hz
0.0020

@Frequency 1.00e+6 Hz
ASTM D150
0.0030

@Frequency 1000 Hz
0.0030

@Frequency 1000 Hz
ASTM D150
0.0040

@Frequency 60.0 Hz
0.0040

@Frequency 60.0 Hz
ASTM D150
Descriptive Properties Value Comments
Hydrogen Transmission 94.5 cc-mm/m²-24hr-atm
ASTM D1434
UV Stability > 2000 hours
ASTM G154
Users viewing this material also viewed the following: