Electrical Properties Metric English Comments
Volume Resistivity 1.20e+17 ohm-cm
1.20e+17 ohm-cm
ASTM D257
Celanese Celanex® 2004-2 PBT  (Unverified Data**)
Celanex 2004-2 is an unfilled polyester that has an excellent combination of flowability and toughness. A typical application for Celanex 2004-2 is electrical connectors containing latches. Celanex ..
Volume Resistivity 1.20e+17 ohm-cm
1.20e+17 ohm-cm
50% RH; ASTM D257
Specialty Coating Systems Parylene D Poly (P-Xylylene) Coating
Parylene D is a polymer of para-xylylene modified by the substitution of chlorine atoms for two of the aromatic hydrogen atoms. Parylene D is similar in properties to Parylene C with the added abili..
Volume Resistivity 1.20e+17 ohm-cm
1.20e+17 ohm-cm
Chengdu Polyster PPHA p-Hydroxybenzoic Acid Polymer
PPHA is difficult to manufacture and brittle as well as low mechanical strength, its compounds have a higher mechanical strength and can be injection moulded. It can work without oil and its perform..
Volume Resistivity 1.20e+17 ohm-cm
1.20e+17 ohm-cm
ASTM D257
DuPont™ Nomex® N196 Paper, 20 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
Volume Resistivity 1.20e+17 ohm-cm
1.20e+17 ohm-cm
ASTM D257
Celanese CELANEX 2004-2 PBT, Unfilled
Celanex 2004-2 is an unfilled polyester that has an excellent combination of flowability and toughness. A typical application for Celanex 2004-2 is electrical connectors containing latches. Celanex ..
Volume Resistivity 1.20e+17 ohm-cm
1.20e+17 ohm-cm
ASTM D257
Celanese Celanex® 3314 PBT, 30% Glass Reinforced
Celanex 3314 is a non-exuding (UL approved V-0 at 1/64 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is w..
Volume Resistivity 1.20e+17 ohm-cm
1.20e+17 ohm-cm
ASTM D257
Celanese Celanex® 602AC PBT, Glass Reinforced
Celanex 602AC is a 10% fiberglass reinforced PBT that has lower warpage and improved impact over standard PBT.To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a ..
Volume Resistivity 1.20e+17 ohm-cm
1.20e+17 ohm-cm
ASTM D257
Celanese Celanex® 3318 PBT, 30% Glass Reinforced
Celanex 3318 is a non-exuding (UL approved V-0 at 1/64 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is w..