Polymer Property : Density = 1.418 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.418 g/cc
0.05123 lb/in³
ASTM D1505
Specialty Coating Systems Parylene D Poly (P-Xylylene) Coating
Parylene D is a polymer of para-xylylene modified by the substitution of chlorine atoms for two of the aromatic hydrogen atoms. Parylene D is similar in properties to Parylene C with the added abili..
Density 1.418 g/cc
0.05123 lb/in³
JIS-Z-8807
Denka VINYKON W2086 PVC, W grade for insulation, for sheaths
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Density 1.418 g/cc
0.05123 lb/in³
JIS-Z-8807
Denka VINYKON R3102 PVC, R grade for hard extrusion
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Density 1.418 g/cc
0.05123 lb/in³
Parylene Coating Services D Poly (P-Xylylene)
Monomer is dichloro para-xylylene. Parylene D is recommended where high temperature resistance is needed; it can be used up to 140°C where oxygen is present.Parylene is a generic name for poly-par..