Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech Royalite R66 PVC/Acrylic Fire Rated Sheet

Category Polymer , Thermoplastic , Acrylic (PMMA) , Vinyl (PVC) , PVC/Acrylic Alloy
Manufacturer Spartech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Royalite R66 PVC/Acrylic Fire Rated Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Fire Rated SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.35 - 1.45 g/cc
1.35 - 1.45 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Flexural Yield Strength 65.5 MPa
9500 psi
ASTM D790
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
73°F; ASTM D256
Impact Test 40.7 J

@Temperature 22.8 °C
30.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 82.8 - 99.0 µm/m-°C

@Temperature 20.0 °C
46.0 - 55.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C
170 °F
ASTM D648
Descriptive Properties Value Comments
Bus and Rail Smoke Rating Dmax < 300
UMTA/DOT/FRA
Flammability Passes
MVSS (Motor Vehicle Safety Standard) 302
Users viewing this material also viewed the following: