Spartech M60095 General Purpose PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Spartech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech M60095 General Purpose PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. Best for clear molding, gaskets, handles and fittings.Information provided by Spartech
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
+.02
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
10 sec ± 3
Tensile Strength, Yield 21.1 MPa
3060 psi
Elongation at Break 290 %
290 %
100% Modulus 0.0174 GPa
2.53 ksi
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F