Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0174 GPa | 2.53 ksi | |
Spartech M60095 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |