Material Notes:
Heat stabilized, low viscosity, injection grade.Information provided by Rhodia; Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ISO 1183-A
Water Absorption 0.72 %

@Time 86400 sec
0.72 %

@Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 230 MPa
33400 psi
ISO 527
Elongation at Break 2.6 %
2.6 %
ISO 527
Tensile Modulus 17.0 GPa
2470 ksi
ISO 527
Flexural Modulus 15.5 GPa
2250 ksi
ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 3146-C
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75-2