Material Notes:
Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black color.Benefits: The product offers an excellent combination between thermal and mechanical properties as well as a low warpage of molded parts.Available in: Asia Pacific, Europe, Latin America and North America.Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applicationsApplications: This grade is commonly used in the automotive industry to mould large parts such as rocker cover and engine covers.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ISO 1183/A
Viscosity 30 cP
<br>@Shear Rate 1000 1/s,<br> Temperature 280 °C
30 cP
<br>@Shear Rate 1000 1/s,<br> Temperature 536 °F
30 cP
<br>@Shear Rate 1000 1/s,<br> Temperature 290 °C
30 cP
<br>@Shear Rate 1000 1/s,<br> Temperature 554 °F
30 cP
<br>@Shear Rate 1000 1/s,<br> Temperature 300 °C
30 cP
<br>@Shear Rate 1000 1/s,<br> Temperature 572 °F
105 cP
<br>@Shear Rate 100 1/s,<br> Temperature 300 °C
105 cP
<br>@Shear Rate 100 1/s,<br> Temperature 572 °F
109 cP
<br>@Shear Rate 100 1/s,<br> Temperature 290 °C
109 cP
<br>@Shear Rate 100 1/s,<br> Temperature 554 °F
120 cP
<br>@Shear Rate 100 1/s,<br> Temperature 280 °C
120 cP
<br>@Shear Rate 100 1/s,<br> Temperature 536 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa
16700 psi
ISO 527 Type 1A
Tensile Stress 22.0 MPa
<br>@Strain 1.00 %,<br> Temperature 120 °C
3190 psi
<br>@Strain 1.00 %,<br> Temperature 248 °F
30.0 MPa
<br>@Strain 1.00 %,<br> Temperature 80.0 °C
4350 psi
<br>@Strain 1.00 %,<br> Temperature 176 °F
45.0 MPa
<br>@Strain 2.00 %,<br> Temperature 120 °C
6530 psi
<br>@Strain 2.00 %,<br> Temperature 248 °F
50.0 MPa
<br>@Strain 1.00 %,<br> Temperature 23.0 °C
7250 psi
<br>@Strain 1.00 %,<br> Temperature 73.4 °F
60.0 MPa
<br>@Strain 2.00 %,<br> Temperature 80.0 °C
8700 psi
<br>@Strain 2.00 %,<br> Temperature 176 °F
60.0 MPa
<br>@Strain 5.00 %,<br> Temperature 120 °C
8700 psi
<br>@Strain 5.00 %,<br> Temperature 248 °F
61.0 MPa
<br>@Strain 8.00 %,<br> Temperature 120 °C
8850 psi
<br>@Strain 8.00 %,<br> Temperature 248 °F
78.0 MPa
<br>@Strain 5.00 %,<br> Temperature 80.0 °C
11300 psi
<br>@Strain 5.00 %,<br> Temperature 176 °F
80.0 MPa
<br>@Strain 8.00 %,<br> Temperature 80.0 °C
11600 psi
<br>@Strain 8.00 %,<br> Temperature 176 °F
130 MPa
<br>@Strain 2.00 %,<br> Temperature 23.0 °C
18900 psi
<br>@Strain 2.00 %,<br> Temperature 73.4 °F
Elongation at Break 3.0 %
3.0 %
ISO 527 Type 1A
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527 Type 1A
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 5.50 J/cm²
26.2 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %