Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 22.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 22.0 MPa

@Strain 1.90 %,
Temperature 40.0 °C
3190 psi

@Strain 1.90 %,
Temperature 104 °F
ISO 527
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers
Tensile Stress 22.0 MPa

@Strain 2.00 %,
Temperature 120 °C
3190 psi

@Strain 2.00 %,
Temperature 248 °F
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY
Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th..
Tensile Stress 22.0 MPa

@Strain 10.0 %,
Temperature 80.0 °C
3190 psi

@Strain 10.0 %,
Temperature 176 °F
Solvay TECHNYL® A 205F PA66, Conditioned
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
Tensile Stress 22.0 MPa

@Strain 20.0 %,
Temperature 120 °C
3190 psi

@Strain 20.0 %,
Temperature 248 °F
Solvay TECHNYL® A 205F PA66, Conditioned
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
Tensile Stress 22.0 MPa

@Strain 1.00 %,
Temperature 120 °C
3190 psi

@Strain 1.00 %,
Temperature 248 °F
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, Conditioned
Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co..
Tensile Stress 22.0 MPa

@Strain 1.71 %,
Temperature 150 °C
3190 psi

@Strain 1.71 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen..
Tensile Stress 22.0 MPa

@Strain 1.90 %,
Temperature 40.0 °C
3190 psi

@Strain 1.90 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)  (Unverified Data**)
Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers
Tensile Stress 22.0 MPa

@Strain 0.180 %,
Temperature 0.000 °C
3190 psi

@Strain 0.180 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
Tensile Stress 22.0 MPa

@Strain 0.531636 %,
Time 360000 sec
3190 psi

@Strain 0.531636 %,
Time 100 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6  (Unverified Data**)
30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 22.0 MPa

@Strain 0.635491 %,
Time 3.60e+7 sec
3190 psi

@Strain 0.635491 %,
Time 10000 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6  (Unverified Data**)
30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 22.0 MPa

@Strain 0.582327 %,
Time 3.60e+6 sec
3190 psi

@Strain 0.582327 %,
Time 1000 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6  (Unverified Data**)
30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 22.0 MPa

@Strain 0.433964 %,
Time 3600 sec
3190 psi

@Strain 0.433964 %,
Time 1.00 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6  (Unverified Data**)
30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 22.0 MPa

@Strain 0.480945 %,
Time 36000 sec
3190 psi

@Strain 0.480945 %,
Time 10.0 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6  (Unverified Data**)
30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 22.0 MPa

@Strain 0.220 %,
Temperature 23.0 °C
3190 psi

@Strain 0.220 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6  (Unverified Data**)
50% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G50HSLA BK416 is a 50% glass fiber reinforced heat stabilized lubricated polyamide 6 resin for injection molding. It has an excellent surface..
Tensile Stress 22.0 MPa

@Strain 50.0 %
3190 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress >= 22.0 MPa

@Strain 100 %
>= 3190 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 772D PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Tensile Stress >= 22.0 MPa

@Strain 300 %
>= 3190 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 695A Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Stress >= 22.0 MPa

@Strain 300 %
>= 3190 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 798A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Copyright © lookpolymers.com All Rights Reserved