Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Veradel® A-100, A-200, A-300 Polyethersulfone  (discontinued **)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Veradel® A-100, A-200, A-300 Polyethersulfone  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.Nov. 2009: Veradel® is the replacement trade name for former Radel® R PESU products.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Water Absorption 0.54 %
0.54 %
in 24 hours per ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 83.0 MPa
12000 psi
ASTM D638
Elongation at Break 40 - 80 %
40 - 80 %
ASTM D638
Elongation at Yield 6.5 %
6.5 %
ASTM D638
Tensile Modulus 2.65 GPa
384 ksi
ASTM D638
Flexural Yield Strength 111 MPa
16100 psi
ASTM D790
Flexural Modulus 2.90 GPa
421 ksi
ASTM D790
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
Tensile Impact Strength 340 kJ/m²
162 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 49.0 µm/m-°C

@Temperature 20.0 °C
27.2 µin/in-°F

@Temperature 68.0 °F
ASTM E381
CTE, linear, Transverse to Flow 49.0 µm/m-°C

@Temperature 20.0 °C
27.2 µin/in-°F

@Temperature 68.0 °F
ASTM E381
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
399 °F
ASTM D648
UL RTI, Electrical 180 °C

@Thickness 1.57 mm
356 °F

@Thickness 0.0618 in
UL RTI, Mechanical with Impact 180 °C

@Thickness 1.57 mm
356 °F

@Thickness 0.0618 in
UL RTI, Mechanical without Impact 180 °C

@Thickness 1.57 mm
356 °F

@Thickness 0.0618 in
Flammability, UL94 V-0

@Thickness 0.600 mm
V-0

@Thickness 0.0236 in
V-0

@Thickness 0.600 mm
V-0

@Thickness 0.0236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.70e+15 ohm-cm
1.70e+15 ohm-cm
ASTM D257
Dielectric Constant 3.5

@Frequency 1000 Hz
3.5

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm

@Thickness 3.30 mm
406 kV/in

@Thickness 0.130 in
ASTM D149
Dissipation Factor 0.0020

@Frequency 1000 Hz
0.0020

@Frequency 1000 Hz
ASTM D150
Users viewing this material also viewed the following: