Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.65 GPa | 384 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML7677A PC (Asia Pacific) Commercial grade for Polycarbonate in only nature color. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E7000 Polyvinyl Chloride, Rigid (PVC, Rigid) 60 degree gloss comparisons: Geon E7000 is 47-49;Geon E7456 is 40-49;Geon E7130 is 38-43;Geon E7370 is 26-31Information provided by PolyOne |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® A-100, A-200, A-300 Polyethersulfone
(discontinued **) For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N.. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | 1 mm/min |
Polimeri Europa SINKRAL B232/E ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EGN,105-04-09-25 Extrusion and thermoforming grade with good thermal resistance, high stiffness and a very low vol.. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Asia Pacific) LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Europe-Africa-Middle East) LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX05305C PC (Asia Pacific) LNP* Stat-kon* DX05305C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Asia Pacific) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl PKN4736 PPE+HIPS (Europe-Africa-Middle East) NORYL PKN4736 is a PPO+HIPS extrusion grade for dilution with polystyrene resin. It is suitable for (microwavable) food packaging and is compliant with US and European food contact regulations.This .. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX05305C PC LNP* STAT-KON* DX05305C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | 1 mm/min; ISO 527-1,-2 |
Covestro Bayblend® FR3005 BBS310 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | 1mm/min; ISO 527-1 |
Denka MALECCA K-400 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide BST01 PA6, Impact Modified, Injection Molded BST01 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | ISO 527 - 1 & - 2 |
Asahi Kasei Tenac®-C 3510 Copolymer Acetal Resin High-impact, high elongation grade, with increased molecular weightInformation provided by Asahi Kasei Corporation. |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | |
Henkel Hysol EA 9330 Paste Adhesive System Easy mix adhesive with high peel strength and excellent environmental durability.Applications: Structural Repair Composite Bonding |
|||
Tensile Modulus | 2.65 GPa | 384 ksi | ISO 527 |
Manifattura Cattaneo POM c+PTFE Acetal, PTFE Filled Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |