Thermal Properties Metric English Comments
UL RTI, Electrical 180 °C

@Thickness 1.57 mm
356 °F

@Thickness 0.0618 in
Solvay Specialty Polymers Veradel® A-100, A-200, A-300 Polyethersulfone  (discontinued **)
For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N..
UL RTI, Electrical 180 °C
356 °F
UL 746B
SABIC Innovative Plastics ULTEM 2300 PEI
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors.
UL RTI, Electrical 180 °C
356 °F
UL 746B
SABIC Innovative Plastics ULTEM 2300 PEI (Asia Pacific)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors.
UL RTI, Electrical 180 °C
356 °F
UL 746B
SABIC Innovative Plastics ULTEM 2300 PEI (Europe-Africa-Middle East)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
UL RTI, Electrical 180 °C
356 °F
UL 746B
SABIC Innovative Plastics ULTEM 2300R PEI
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
UL RTI, Electrical 180 °C
356 °F
UL 746B
SABIC Innovative Plastics ULTEM 2300R PEI (Asia Pacific)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
UL RTI, Electrical 180 °C
356 °F
UL 746B
SABIC Innovative Plastics ULTEM 2300R PEI (Europe-Africa-Middle East)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
UL RTI, Electrical 180 °C
356 °F
UL 746B
SABIC Innovative Plastics ULTEM 2310 PEI
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
UL RTI, Electrical 180 °C
356 °F
UL 746B
SABIC Innovative Plastics ULTEM 2310 PEI (Asia Pacific)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
UL RTI, Electrical 180 °C
356 °F
UL 746B
SABIC Innovative Plastics ULTEM 2310 PEI (Europe-Africa-Middle East)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
UL RTI, Electrical 180 °C
356 °F
UL 746B
SABIC Innovative Plastics ULTEM 2310R PEI
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
UL RTI, Electrical 180 °C
356 °F
UL 746B
SABIC Innovative Plastics ULTEM 2310R PEI (Asia Pacific)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
UL RTI, Electrical 180 °C
356 °F
UL 746B
SABIC Innovative Plastics ULTEM 2310R PEI (Europe-Africa-Middle East)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
UL RTI, Electrical 180 °C
356 °F
UL 746B
SABIC Innovative Plastics ULTEM 3452 PEI
45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.
UL RTI, Electrical 180 °C
356 °F
UL 746B
SABIC Innovative Plastics ULTEM 3452 PEI (Asia Pacific)
45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.
UL RTI, Electrical 180 °C
356 °F
50% decrease of tensile strength after 20000h; 746B
BASF Ultrason E 2010 G4 20% Glass Filled PES
Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.