Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers FOMBLIN® Y06/6 PFPE Lubricant

Category Fluid , Lubricant , Perfluoropolyether (PFPE)
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name FOMBLIN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers FOMBLIN® Y06/6 PFPE Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporative loss; and good viscosity indices.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.88 g/cc
0.0679 lb/in³
ASTM D891
Viscosity Measurement 70
70
Viscosity Index; ASTM D2270
Kinematic Viscosity 60 cSt

@Temperature 20.0 °C
60 cSt

@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 3.9 cSt
3.9 cSt
ASTM D445
Molecular Weight 1800 g/mol
1800 g/mol
Evaporation Loss 6.0 %
6.0 %
22 hrs. at 120°C; ASTM 2595
20 %
20 %
22 hrs. at 149°C; ASTM 2595
Surface Tension 21 dynes/cm
21 dynes/cm
ASTM D1331
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 107 kg
236 lb (mass)
Mean Hertz Load; IP 239
282 kg
622 lb (mass)
Init. Seiz. Load; IP 239
398 kg
878 lb (mass)
Welding Load; IP 239
Four Ball Wear 0.630 mm
0.0248 in
Avg. scar diameter; ASTM D4172
Thermal Properties Metric English Comments
Pour Point -50.0 °C
-58.0 °F
ASTM D97
Descriptive Properties Value Comments
Approximate ISO Grade 22
Users viewing this material also viewed the following: