Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 21 dynes/cm | 21 dynes/cm | ASTM D1331 |
Solvay Specialty Polymers FOMBLIN® Y L-VAC 06/6 PFPE Pump Oil FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and.. |
|||
Surface Tension | 21 dynes/cm | 21 dynes/cm | ASTM D1331 |
Solvay Specialty Polymers FOMBLIN® Y04 PFPE Lubricant FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati.. |
|||
Surface Tension | 21 dynes/cm | 21 dynes/cm | ASTM D1331 |
Solvay Specialty Polymers FOMBLIN® Y06/6 PFPE Lubricant FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati.. |
|||
Surface Tension | 21 dynes/cm | 21 dynes/cm | |
Dow Corning XIAMETER® PMCPPMX-200 200CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 200CS. 100% active, 200 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |