Physical Properties Metric English Comments
Kinematic Viscosity 60 cSt

@Temperature 20.0 °C
60 cSt

@Temperature 68.0 °F
ASTM D445
Solvay Specialty Polymers FOMBLIN® Y06/6 PFPE Lubricant
FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati..