Kinematic Viscosity at 100°C (212°F) 3.9 cSt
3.9 cSt
ASTM D445
Solvay Specialty Polymers FOMBLIN® Y06/6 PFPE Lubricant
FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati..