Solvay Specialty Polymers FOMBLIN® Y04 PFPE Lubricant

Category Fluid , Lubricant , Perfluoropolyether (PFPE)
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name FOMBLIN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers FOMBLIN® Y04 PFPE Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporative loss; and good viscosity indices.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.87 g/cc
0.0676 lb/in³
ASTM D891
Viscosity Measurement 60
60
Viscosity Index; ASTM D2270
Kinematic Viscosity 38 cSt

@Temperature 20.0 °C
38 cSt

@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 15 cSt
15 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 3.2 cSt
3.2 cSt
ASTM D445
Molecular Weight 1500 g/mol
1500 g/mol
Evaporation Loss 14 %
14 %
22 hrs. at 120°C; ASTM 2595
Surface Tension 21 dynes/cm
21 dynes/cm
ASTM D1331
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 84.0 kg
185 lb (mass)
Mean Hertz Load; IP 239
224 kg
494 lb (mass)
Init. Seiz. Load; IP 239
355 kg
783 lb (mass)
Welding Load; IP 239
Four Ball Wear 0.510 mm
0.0201 in
Avg. scar diameter; ASTM D4172
Thermal Properties Metric English Comments
Pour Point -58.0 °C
-72.4 °F
ASTM D97
Descriptive Properties Value Comments
Approximate ISO Grade 15