Thermal Properties Metric English Comments
Pour Point -58.0 °C
-72.4 °F
Base Oil; ASTM D97
Nye Lubricants 380 (RL) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -58.0 °C
-72.4 °F
Base Oil; ASTM D97
Nye Lubricants 380C (RL) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -58.0 °C
-72.4 °F
Base Oil; ASTM D97
Nye Lubricants 380G1 (RL) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -58.0 °C
-72.4 °F
ASTM D97
Solvay Specialty Polymers FOMBLIN® Y04 PFPE Lubricant
FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati..