Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 355 kg | 783 lb (mass) | Welding Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® Y04 PFPE Lubricant FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati.. |
|||
Four Ball Extreme Pressure, Weld Load | 355 kg | 783 lb (mass) | Init. Seiz. Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® YPL1500 PFPE Lubricant FOMBLIN YR perfluoropolyether fluids have excellent high temperature stability, good low temperature properties, very good E.P. and wear characteristics, good evaporative loss, and good viscosity in.. |