Material Notes:
Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental
Physical Properties Metric English Comments
Density 11.6 g/cc
0.419 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 250
250
HV5/30; after porcelain firing
250
250
HV5/30; hardened
Tensile Strength, Yield 520 MPa

@Strain 0.200 %
75400 psi

@Strain 0.200 %
after porcelain firing
520 MPa

@Strain 0.200 %
75400 psi

@Strain 0.200 %
hardened
Elongation at Break 27 %
27 %
after porcelain firing
27 %
27 %
hardened
Modulus of Elasticity 116 GPa
16800 ksi
Thermal Properties Metric English Comments
CTE, linear 14.1 µm/m-°C

@Temperature 25.0 - 500 °C
7.83 µin/in-°F

@Temperature 77.0 - 932 °F
Component Elements Properties Metric English Comments
Gallium, Ga 6.5 %
6.5 %
Germanium, Ge 0.10 %
0.10 %
Gold, Au 6.0 %
6.0 %
Palladium, Pd 75 %
75 %
Ruthenium, Ru 0.50 %
0.50 %
Silver, Ag 8.4 %
8.4 %
Tin, Sn 3.5 %
3.5 %
Processing Properties Metric English Comments
Processing Temperature 849 °C
1560 °F
Preheating Temp.
Melt Temperature 1110 - 1280 °C
2030 - 2340 °F
Casting Temperature 1400 °C
2550 °F
Descriptive Properties Value Comments
Color white
Users viewing this material also viewed the following: