Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Engineered Polymers DEXPRO® R120 TPV - High-Impact Polypropylene  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV) , Polypropylene (PP)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Engineered Polymers DEXPRO® R120 TPV - High-Impact Polypropylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: DEXPRO® R120 is a reactor-grade thermoplastic elastomeric olefin resin with a good balance of impact performance, stiffness, and paintability. Applications: Painted bumper fasciasInformation provided by Solvay Engineered Polymers. LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ISO 1183
Linear Mold Shrinkage 0.011 - 0.014 cm/cm
0.011 - 0.014 in/in
as molded; ISO 294
0.015 - 0.018 cm/cm
0.015 - 0.018 in/in
after bake; ISO 294
Melt Flow 25.5 g/10 min
25.5 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 0.850 GPa
123 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test 20.0 J
14.8 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 11.8 µm/m-°C

@Temperature -30.0 - 80.0 °C
6.56 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228