Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.8 µm/m-°C @Temperature 20.0 °C |
6.56 µin/in-°F @Temperature 68.0 °F |
|
Hogen Duralloy H1W 55 Tungsten/45 Copper PM Metal Composite RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 20.0 °C |
6.56 µin/in-°F @Temperature 68.0 °F |
|
MMCC Aluminum/SiC 55p Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 100 °C |
6.56 µin/in-°F @Temperature 77.0 - 212 °F |
ASTM E831 |
M Cubed Technologies MMC-S55 Aluminum alloy-55% SiC Metal Matrix Composite High stiffness, low density composite. Parts are cast using several standard foundry techniques Size range varies from small components (1lb or smaller) to parts greater than 10 ft. square with co.. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 20.0 °C |
6.56 µin/in-°F @Temperature 68.0 °F |
|
California Fine Wire Stablohm 812 Chromium, Aluminum, and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature -30.0 - 80.0 °C |
6.56 µin/in-°F @Temperature -22.0 - 176 °F |
ASTM E228 |
Solvay Engineered Polymers DEXPRO® R120 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R120 is a reactor-grade thermoplastic elastomeric olefin resin with a good balance of impact performance, stiffness, and paintability. Applications: Painted bumper fasciasInfor.. |