Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Chemicals E2000 Methylene chloride

Category Fluid , Solvent
Manufacturer Solvay Chemicals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals E2000 Methylene chloride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thanks to its specific characteristics, especially high solvent power, it is used where a high-grade economic solvent is required, because it successfully dissolves many organic compounds. Its high volatility is especially recommended to extract materials sensitive towards temperatureEINECS Number: 200-838-9/CAS Number: 75-09-2/UN number: 1593Information provided by Solvay
Physical Properties Metric English Comments
Density 1.318 - 1.329 g/cc
0.04762 - 0.04801 lb/in³
D<sub>20/4</sub>
1.32 - 1.332 g/cc
0.0477 - 0.04812 lb/in³
D<sub>20/20</sub>
1.288 g/cc

@Temperature 40.0 °C
0.04653 lb/in³

@Temperature 104 °F
1.297 g/cc

@Temperature 35.0 °C
0.04686 lb/in³

@Temperature 95.0 °F
1.306 g/cc

@Temperature 30.0 °C
0.04718 lb/in³

@Temperature 86.0 °F
1.316 g/cc

@Temperature 25.0 °C
0.04754 lb/in³

@Temperature 77.0 °F
1.325 g/cc

@Temperature 20.0 °C
0.04787 lb/in³

@Temperature 68.0 °F
1.334 g/cc

@Temperature 15.0 °C
0.04819 lb/in³

@Temperature 59.0 °F
1.343 g/cc

@Temperature 10.0 °C
0.04852 lb/in³

@Temperature 50.0 °F
1.352 g/cc

@Temperature 5.00 °C
0.04884 lb/in³

@Temperature 41.0 °F
1.361 g/cc

@Temperature 0.000 °C
0.04917 lb/in³

@Temperature 32.0 °F
Viscosity 0.30 cP

@Temperature 30.0 °C
0.30 cP

@Temperature 86.0 °F
Dynamic
0.36 cP

@Temperature 40.0 °C
0.36 cP

@Temperature 104 °F
Dynamic
0.38 cP

@Temperature 35.0 °C
0.38 cP

@Temperature 95.0 °F
Dynamic
0.41 cP

@Temperature 25.0 °C
0.41 cP

@Temperature 77.0 °F
Dynamic
0.43 cP

@Temperature 20.0 °C
0.43 cP

@Temperature 68.0 °F
Dynamic
0.46 cP

@Temperature 15.0 °C
0.46 cP

@Temperature 59.0 °F
Dynamic
0.48 cP

@Temperature 10.0 °C
0.48 cP

@Temperature 50.0 °F
Dynamic
0.51 cP

@Temperature 5.00 °C
0.51 cP

@Temperature 41.0 °F
Dynamic
0.53 cP

@Temperature 0.000 °C
0.53 cP

@Temperature 32.0 °F
Dynamic
Molecular Weight 84.9 g/mol
84.9 g/mol
Vapor Pressure 0.189 bar

@Temperature 0.000 °C
142 torr

@Temperature 32.0 °F
0.241 bar

@Temperature 5.00 °C
181 torr

@Temperature 41.0 °F
0.304 bar

@Temperature 10.0 °C
228 torr

@Temperature 50.0 °F
0.379 bar

@Temperature 15.0 °C
284 torr

@Temperature 59.0 °F
0.469 bar

@Temperature 20.0 °C
352 torr

@Temperature 68.0 °F
0.575 bar

@Temperature 25.0 °C
431 torr

@Temperature 77.0 °F
0.700 bar

@Temperature 30.0 °C
525 torr

@Temperature 86.0 °F
0.847 bar

@Temperature 35.0 °C
635 torr

@Temperature 95.0 °F
1.016 bar

@Temperature 40.0 °C
762.1 torr

@Temperature 104 °F
Descriptive Properties Value Comments
Appearance Clear without suspended matter
ASMT D3741/B
Color <10
APHA
Composition <1 mg/kg
Oxidizing Compounds (Cl2)
<1 mg/kg
Heavy Metals* (Pb)
<100 mg/kg
1,2-Dichloroethane
<100 mg/kg
1,1-Dichloroethylene
<12 mg/kg
Carbon Tetrachloride
<5 mg/kg
Acidity (HCl)
<50 mg/kg
Moisture (H2O), Karl Fischer, ASTM E1064
<56 mg/kg
Chloroform
1500-2500 mg/kg
Stabilizer (Ethanol)
Purity >999.5 g/kg
without stabilizers
Users viewing this material also viewed the following: