Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.361 g/cc @Temperature 0.000 °C |
0.04917 lb/in³ @Temperature 32.0 °F |
|
Solvay Chemicals A50 Methylene chloride Thanks to its specific characteristics, especially high solvent power, it is used where a high-grade economic solvent is required, because it successfully dissolves many organic compounds. Its high .. |
|||
Density | 1.361 g/cc @Temperature 0.000 °C |
0.04917 lb/in³ @Temperature 32.0 °F |
|
Solvay Chemicals E2000 Methylene chloride Thanks to its specific characteristics, especially high solvent power, it is used where a high-grade economic solvent is required, because it successfully dissolves many organic compounds. Its high .. |
|||
Density | 1.361 g/cc | 0.04917 lb/in³ | JIS-Z-8807 |
Denka VINYKON R5205 PVC, R grade for hard extrusion A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |