Polymer Property : Viscosity = 0.38 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 0.38 cP

@Temperature 329 °C
0.38 cP

@Temperature 625 °F
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid
Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and..
Viscosity 0.38 cP

@Temperature 35.0 °C
0.38 cP

@Temperature 95.0 °F
Dynamic
Solvay Chemicals A50 Methylene chloride
Thanks to its specific characteristics, especially high solvent power, it is used where a high-grade economic solvent is required, because it successfully dissolves many organic compounds. Its high ..
Viscosity 0.38 cP

@Temperature 35.0 °C
0.38 cP

@Temperature 95.0 °F
Dynamic
Solvay Chemicals E2000 Methylene chloride
Thanks to its specific characteristics, especially high solvent power, it is used where a high-grade economic solvent is required, because it successfully dissolves many organic compounds. Its high ..
Viscosity 0.38 cP

@Temperature 100 °C
0.38 cP

@Temperature 212 °F
Dynamic, Concentration 0.15 kg FeCl3/kg
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (11 wt% - 20 wt% Concentration)
Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regene..
Viscosity 0.38 cP

@Temperature 80.0 °C
0.38 cP

@Temperature 176 °F
Dynamic, Concentration 0.05 kg FeCl3/kg
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (2 wt% - 10 wt% Concentration)
Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regene..