Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.41 cP @Temperature 316 °C |
0.41 cP @Temperature 600 °F |
|
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and.. |
|||
Viscosity | 0.41 cP @Temperature 25.0 °C |
0.41 cP @Temperature 77.0 °F |
Dynamic |
Solvay Chemicals A50 Methylene chloride Thanks to its specific characteristics, especially high solvent power, it is used where a high-grade economic solvent is required, because it successfully dissolves many organic compounds. Its high .. |
|||
Viscosity | 0.41 cP @Temperature 25.0 °C |
0.41 cP @Temperature 77.0 °F |
Dynamic |
Solvay Chemicals E2000 Methylene chloride Thanks to its specific characteristics, especially high solvent power, it is used where a high-grade economic solvent is required, because it successfully dissolves many organic compounds. Its high .. |
|||
Viscosity | 0.41 cP @Temperature 80.0 °C |
0.41 cP @Temperature 176 °F |
Dynamic, Concentration 0.10 kg FeCl3/kg |
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (2 wt% - 10 wt% Concentration) Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regene.. |
|||
Viscosity | 0.41 cP @Temperature 110 °C |
0.41 cP @Temperature 230 °F |
Dynamic |
Solvay Chemicals Perchloroethylene Perchloroethylene is a non-flammable productEINECS Number: 204-825-9/CAS Number: 127-18-4/UN number: 1897Information provided by Solvay |