Polymer Property : Vapor Pressure = 284 torr Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.379 bar

@Temperature 15.0 °C
284 torr

@Temperature 59.0 °F
Solvay Chemicals A50 Methylene chloride
Thanks to its specific characteristics, especially high solvent power, it is used where a high-grade economic solvent is required, because it successfully dissolves many organic compounds. Its high ..
Vapor Pressure 0.379 bar

@Temperature 15.0 °C
284 torr

@Temperature 59.0 °F
Solvay Chemicals E2000 Methylene chloride
Thanks to its specific characteristics, especially high solvent power, it is used where a high-grade economic solvent is required, because it successfully dissolves many organic compounds. Its high ..