Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 7845TL Laser Toner Printable Polyester Label Material

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7845TL Laser Toner Printable Polyester Label Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Laser Toner Printable Polyester Label Material 7845TL is a matte clear polyester designed for sheet fed laser imprinting. This label material utilizes 3M™ Adhesive 310 which provides firmness and high precision strength on a variety of surfaces including HSE plastics and metals.Information provided by 3M
Mechanical Properties Metric English Comments
Peel Strength 0.05478 kN/m
0.3125 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.0877 kN/m
0.500 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.131 kN/m
0.750 pli
LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.175 kN/m
1.00 pli
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.175 kN/m
1.00 pli
HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.1972 kN/m
1.125 pli
Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.1972 kN/m
1.125 pli
Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.219 kN/m
1.25 pli
LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.219 kN/m
1.25 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.219 kN/m
1.25 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.219 kN/m
1.25 pli
LD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.2410 kN/m
1.375 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.263 kN/m
1.50 pli
HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.263 kN/m
1.50 pli
Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.263 kN/m
1.50 pli
LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.29582 kN/m
1.6875 pli
Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.29582 kN/m
1.6875 pli
HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.3287 kN/m
1.875 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.3287 kN/m
1.875 pli
Polypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.351 kN/m
2.00 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.351 kN/m
2.00 pli
Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.351 kN/m
2.00 pli
Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.36156 kN/m
2.0625 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.3725 kN/m
2.125 pli
Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.38347 kN/m
2.1875 pli
HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.38347 kN/m
2.1875 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.38347 kN/m
2.1875 pli
Polypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.40538 kN/m
2.3125 pli
Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.4163 kN/m
2.375 pli
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.438 kN/m
2.50 pli
Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.44921 kN/m
2.5625 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.44921 kN/m
2.5625 pli
Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.4602 kN/m
2.625 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.47112 kN/m
2.6875 pli
Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.47112 kN/m
2.6875 pli
Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.5040 kN/m
2.875 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.5040 kN/m
2.875 pli
Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.51494 kN/m
2.9375 pli
Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.51494 kN/m
2.9375 pli
Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.570 kN/m
3.25 pli
Glass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.570 kN/m
3.25 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.657 kN/m
3.75 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.6793 kN/m
3.875 pli
Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.7231 kN/m
4.125 pli
Glass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.745 kN/m
4.25 pli
Glass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.745 kN/m
4.25 pli
Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.8108 kN/m
4.625 pli
Stainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
1.49 kN/m
8.50 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Copyright © lookpolymers.com All Rights Reserved