Shuman SP810 Black Polystyrene High Impact

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Shuman
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shuman SP810 Black Polystyrene High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good impact strength, easy processability, good surface appearance, ULInformation provided by Shuman Plastics, Inc.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Melt Flow 4.0 - 8.0 g/10 min
4.0 - 8.0 g/10 min
multiple ranges available; ASTM D1238
6.0 - 10 g/10 min
6.0 - 10 g/10 min
ASTM D1238
8.0 - 12 g/10 min
8.0 - 12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell L 60
60
ASTM D785
Tensile Strength 30.36 MPa
4404 psi
ASTM D638
Izod Impact, Notched >= 0.961 J/cm
>= 1.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 79.6 µm/m-°C
44.2 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ASTM D648
Vicat Softening Point 97.2 °C
207 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 1.57 mm
HB

@Thickness 0.0618 in
Processing Properties Metric English Comments
Processing Temperature 204 - 227 °C
400 - 440 °F