Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shuman FR380 Grey PC/ABS Alloy, Flame Retardant

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant
Manufacturer Shuman
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shuman FR380 Grey PC/ABS Alloy, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Melt Flow 4.0 - 10 g/10 min
4.0 - 10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 48.3 MPa
7000 psi
ASTM D638
Flexural Modulus 2.21 - 2.62 GPa
320 - 380 ksi
ASTM D790
Izod Impact, Notched 4.00 - 5.61 J/cm

@Thickness 3.17 mm
7.50 - 10.5 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 1.57 mm
V-0

@Thickness 0.0618 in
Processing Properties Metric English Comments
Processing Temperature 238 - 277 °C
460 - 530 °F
Drying Temperature 79.4 - 110 °C

@Time 10800 - 14400 sec
175 - 230 °F

@Time 3.00 - 4.00 hour
Dehumidifying Dryer