Mechanical Properties Metric English Comments
Izod Impact, Notched 4.00 J/cm

@Temperature 23.0 °C
7.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products F4702-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Exterior door moldingsRigid bumper coversInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 4.00 J/cm

@Temperature 23.0 °C
7.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products FT4702-527UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic
Applications: Exterior door moldingsRigid bumper coversBodyside claddings and fairingsAutomotive grillesInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 4.00 J/cm

@Temperature 23.0 °C
7.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products FT4702-698UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black
Applications: Bumper trimExterior componentsDoor claddingsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 4.00 J/cm

@Temperature 23.0 °C
7.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products FT4702-715UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey
Applications: Exterior componentsGrillesBumper trimDoor componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 4.00 - 5340 J/cm
7.50 - 10000 ft-lb/in
Average value: 13.0 J/cm Grade Count:29
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Izod Impact, Notched 4.00 J/cm
7.50 ft-lb/in
MTI ThermoStran® PA66-50G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Izod Impact, Notched 4.00 J/cm
7.50 ft-lb/in
73°F; ASTM D256
Spartech Royalite R24 ABS General Purpose Sheet
Description: General Purpose SheetInformation provided by Spartech.
Izod Impact, Notched 4.00 J/cm
7.50 ft-lb/in
73°F; ASTM D256
Spartech Royalite R26 ABS General Purpose Sheet
Description: General Purpose SheetInformation provided by Spartech.
Izod Impact, Notched 4.00 - 5.61 J/cm

@Thickness 3.17 mm
7.50 - 10.5 ft-lb/in

@Thickness 0.125 in
ASTM D256
Shuman 310 Utility Black PC/ABS Alloy
Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc.
Izod Impact, Notched 4.00 - 5.61 J/cm

@Thickness 3.17 mm
7.50 - 10.5 ft-lb/in

@Thickness 0.125 in
ASTM D256
Shuman 330 White PC/ABS Alloy
Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc.
Izod Impact, Notched 4.00 - 5.61 J/cm

@Thickness 3.17 mm
7.50 - 10.5 ft-lb/in

@Thickness 0.125 in
ASTM D256
Shuman 380 Grey PC/ABS Alloy
Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc.
Izod Impact, Notched 4.00 - 5.61 J/cm

@Thickness 3.17 mm
7.50 - 10.5 ft-lb/in

@Thickness 0.125 in
ASTM D256
Shuman FR310 Utility Black PC/ABS Alloy, Flame Retardant
Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shum..
Izod Impact, Notched 4.00 - 5.61 J/cm

@Thickness 3.17 mm
7.50 - 10.5 ft-lb/in

@Thickness 0.125 in
ASTM D256
Shuman FR380 Grey PC/ABS Alloy, Flame Retardant
Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shum..
Izod Impact, Notched 4.00 J/cm
7.50 ft-lb/in
-20°F; ASTM D256
Styron Pulse® 2200BG ABS + PC
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Izod Impact, Notched 4.00 J/cm
7.50 ft-lb/in
ASTM D256
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform..
Izod Impact, Notched 4.00 J/cm
7.50 ft-lb/in
ASTM D256
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform..
Izod Impact, Notched 4.00 J/cm
7.50 ft-lb/in
ASTM D256
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform..
Izod Impact, Notched 4.00 J/cm
7.50 ft-lb/in
ASTM D256
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform..
Izod Impact, Notched 4.00 J/cm
7.50 ft-lb/in
ASTM D256
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform..
Izod Impact, Notched 4.00 J/cm
7.50 ft-lb/in
ASTM D256
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform..
Izod Impact, Notched 4.00 J/cm
7.50 ft-lb/in
LAB034
ExxonMobil Mytex™ AS65KW-1ATM
Talc filled compounded polypropylene produced for automotive interior applicationsInformation provided by ExxonMobil Chemical
Izod Impact, Notched 4.00 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
7.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
bar; ASTM D256
Diamond Polymers ABS 7500E
Description: Extrusion Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
Izod Impact, Notched 4.00 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
7.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
bar; ASTM D256
Diamond Polymers ABS 7502
Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
Izod Impact, Notched 4.00 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
7.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
bar; ASTM D256
Diamond Polymers ABS VP-11 ELG
Description: Extrusion Grade, Low Gloss, Flame RetardantInformation provided by Diamond Polymers, Inc.
Izod Impact, Notched 4.00 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
7.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
bar; ASTM D256
Diamond Polymers ABS 7501
Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
Izod Impact, Notched 4.00 J/cm
7.50 ft-lb/in
ASTM D256