Shin-Etsu Silicones FE-273U Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones FE-273U Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FE-273U is high modulus and low compression set fluorosilicone compounds. It is designed to process well in modling application.FeaturesExcellent fuel and solvent resistanceUsable over a broad temperature rangeAccepts extending fillers for compounding to higher durometersApplicationsChemical resistant packings and sealsOil and fuel resistant seals, O rings, diaphragms for automotiveHeat and cold resistant packings, gaskets for aeronauticalInformation Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
Tensile Strength 9.58 MPa
1390 psi
Elongation at Yield 240 %
240 %
100% Modulus 0.00390 GPa
0.566 ksi
Tear Strength 18.1 kN/m
103 pli
Compression Set 5.0 %

@Temperature 180 °C,
Time 79200 sec
5.0 %

@Temperature 356 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 200 °C
4.00 hour

@Temperature 392 °F
Post Cure