Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00390 GPa | 0.566 ksi | ISO 37 |
Termopol Termoton® K2GA3060A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
100% Modulus | 0.00390 GPa | 0.565 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 81A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
100% Modulus | 0.00390 GPa | 0.566 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N330 (HAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00390 GPa | 0.566 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Talc-Mistron Vapor MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00390 GPa | 0.566 ksi | DIN 53504 |
Huntsman IROGRAN® A 65 P 4324 N TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
100% Modulus | 0.00390 GPa | 0.566 ksi | |
Taiwan PU Corporation TPUI-L75 Low Temperature Resistance, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00390 GPa | 0.566 ksi | |
Shin-Etsu Silicones FE-273U Elastomer FE-273U is high modulus and low compression set fluorosilicone compounds. It is designed to process well in modling application.FeaturesExcellent fuel and solvent resistanceUsable over a broad temp.. |
|||
100% Modulus | 0.00390 GPa | 0.566 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 4175 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4175 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
100% Modulus | 0.00390 GPa | 0.566 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 4475 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4475 is a medium hardness grade possessing exceptional tensile strength, superior compressio.. |
|||
100% Modulus | 0.00390 GPa | 0.566 ksi | NBR Conductive Hose Compound |
TIMCAL ENSACO™ 250G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
100% Modulus | 0.00390 GPa | 0.566 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N330 (HAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00390 GPa | 0.566 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Talc-Mistron Vapor MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00390 GPa | 0.566 ksi | ASTM D412 |
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H.. |
|||
100% Modulus | 0.00390 GPa | 0.565 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 81A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
100% Modulus | 0.00390 GPa | 0.566 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4770P General Purpose Compound FormulationNordel® IP 4770P |
|||
100% Modulus | 0.00390 GPa | 0.566 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4770R General Purpose Compound FormulationNordel® IP 4770R |
|||
100% Modulus | 0.00390 GPa | 0.566 ksi | Cured 7 min at 177°C and Post Cured 2 hr at 232°C |
DuPont Performance Polymers VTR 8505/8500 Formulation
(discontinued **) FormulationViton® 8505 |