Polymer Property : 100% Modulus = 0.566 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00390 GPa
0.566 ksi
ISO 37
Termopol Termoton® K2GA3060A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
100% Modulus 0.00390 GPa
0.566 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N330 (HAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00390 GPa
0.566 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Talc-Mistron Vapor
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00390 GPa
0.566 ksi
DIN 53504
Huntsman IROGRAN® A 65 P 4324 N TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
100% Modulus 0.00390 GPa
0.566 ksi
Taiwan PU Corporation TPUI-L75 Low Temperature Resistance, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
100% Modulus 0.00390 GPa
0.566 ksi
Shin-Etsu Silicones FE-273U Elastomer
FE-273U is high modulus and low compression set fluorosilicone compounds. It is designed to process well in modling application.FeaturesExcellent fuel and solvent resistanceUsable over a broad temp..
100% Modulus 0.00390 GPa
0.566 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 4175 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4175 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical..
100% Modulus 0.00390 GPa
0.566 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 4475 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4475 is a medium hardness grade possessing exceptional tensile strength, superior compressio..
100% Modulus 0.00390 GPa
0.566 ksi
NBR Conductive Hose Compound
TIMCAL ENSACO™ 250G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..
100% Modulus 0.00390 GPa
0.566 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N330 (HAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00390 GPa
0.566 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Talc-Mistron Vapor
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00390 GPa
0.566 ksi
ASTM D412
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane
Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H..
100% Modulus 0.00390 GPa
0.566 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4770P General Purpose Compound
FormulationNordel® IP 4770P
100% Modulus 0.00390 GPa
0.566 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4770R General Purpose Compound
FormulationNordel® IP 4770R
100% Modulus 0.00390 GPa
0.566 ksi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
DuPont Performance Polymers VTR 8505/8500 Formulation  (discontinued **)
FormulationViton® 8505