Shakespeare WonderThread® SN-40 ultra soft TEX# 18 Nylon Industrial Sewing Thread

Category Polymer , Thermoplastic , Nylon
Manufacturer Shakespeare Company
Trade Name WonderThread®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare WonderThread® SN-40 ultra soft TEX# 18 Nylon Industrial Sewing Thread.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided by Shakespeare Company.
Physical Properties Metric English Comments
Fiber Count 200 dtex
180 denier
Mechanical Properties Metric English Comments
Tensile Strength at Break 539 MPa
78200 psi
2.21 lb. load and 0.006 in. diameter
Elongation at Yield 8.0 - 15 %
8.0 - 15 %
at 1.75 G/D
Tenacity 0.494 N/tex
5.60 g/denier
2.21 lb. load
Thermal Properties Metric English Comments
Shrinkage 0.00 - 4.0 %
0.00 - 4.0 %
3 min. in Boiling Water