S&E Specialty Polymers TufFill NH™ 2102A PP, Flame Retardant

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer S&E Specialty Polymers
Trade Name TufFill NH™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufFill NH™ 2102A PP, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: A polypropylene based, zero halogen, flame retardant compound with antistatic properties designed for packaging applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Melt Flow 13.0 g/10 min
13.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.5 MPa
2390 psi
ASTM D638
Tensile Strength, Yield 23.1 MPa
3350 psi
ASTM D638
Elongation at Break >= 58.0 %
>= 58.0 %
ASTM D638
Flexural Modulus 1.68 GPa
244 ksi
tangent; ASTM D790
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256
Dart Drop Total Energy 1.44 J/cm
0.00270 ft-lb/mil
ASTM D5420
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Electrical Properties Metric English Comments
Surface Resistance 1.50e+11 ohm
1.50e+11 ohm
ASTM D257