Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.494 N/tex | 5.60 g/denier | 2.21 lb. load |
Shakespeare WonderThread® SN-40 ultra soft TEX# 18 Nylon Industrial Sewing Thread Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b.. |
|||
Tenacity | 0.494 N/tex | 5.60 g/denier | Line Strength |
UBE 5034MT2 Nylon 6/66 Monofilament (Drawing Ratio=5.5) Specialties: Monomer containing type of 5034T, High softness Applications: Small-big size sport fishing line and long line (main line), Softness required applicationsInformation provided by UBE. |