3M Dyneon™ TF 4246 PTFE 35% Electrocarbon Filled  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Conductive Carbon Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ TF 4246 PTFE 35% Electrocarbon Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon.
Physical Properties Metric English Comments
Density 2.07 g/cc
0.0748 lb/in³
Sintered moldings; ASTM D4894/D4895
Apparent Bulk Density 0.730 g/cc
0.0264 lb/in³
DIN 53 466
Linear Mold Shrinkage 0.022 cm/cm

@Thickness 80.0 mm
0.022 in/in

@Thickness 3.15 in
sheet; ASTM D4894
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ASTM D2240
Tensile Strength, Ultimate 11.0 MPa

@Thickness 2.00 mm
1600 psi

@Thickness 0.0787 in
ASTM D4894
Elongation at Break 50 %

@Thickness 2.00 mm
50 %

@Thickness 0.0787 in
ASTM D4894