Shakespeare Isocorâ„¢ 637 Nylon 6 Terpolymer

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Shakespeare Company
Trade Name Isocor™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare Isocorâ„¢ 637 Nylon 6 Terpolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Isocorâ„¢ 637 multi-polymer is a linear polyamide with unique solubility characteristics and physical properties. Unlike conventional polyamides, Isocorâ„¢ 637 is soluble in common alcohols or in alcohol/water mixtures. Isocorâ„¢ 637 is easily processed and has a wide range of applications due to its physical properties, chemical resistance, and lower melt temperatures. Used for thread bonding, specialty coatings, pigment carriers, specialty adhesives, and polymer additives.Information provided by Shakespeare Company.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D 792
Water Absorption 3.5 %
3.5 %
24 hour immersion; ASTM D 570
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ASTM D 2240
Tensile Strength, Yield 48.0 MPa
6960 psi
ASTM D 638
Elongation at Break 360 %
360 %
ASTM D 638
Flexural Modulus 0.179 GPa
26.0 ksi
ASTM D 790
Thermal Properties Metric English Comments
Melting Point 145 °C
293 °F
DSC
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D 257