Material Notes:
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plastics to low hardness rubber. It is a kind of thermoplastic elastomer, which can be molded with general plastic mold by plasticizing at high temperature.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hour; ASTM D570
Linear Mold Shrinkage 0.022 cm/cm
0.022 in/in
ASTM D955
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 77
77
ASTM D2240
Tensile Strength, Ultimate 49.0 MPa
7110 psi
ASTM D638
Tensile Strength, Yield 29.4 MPa

@Strain 5.00 %
4270 psi

@Strain 5.00 %
ASTM D638
39.2 MPa

@Strain 10.0 %
5690 psi

@Strain 10.0 %
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Flexural Modulus 0.883 GPa
128 ksi
ASTM D790
Izod Impact, Notched 0.392 J/cm
0.735 ft-lb/in
ASTM D256
Tear Strength 260 kN/m
1480 pli
ASTM D1004
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 156 °C
313 °F
ASTM D648