Schott Glass 8652 Sealing Glass

Category Ceramic , Glass
Manufacturer Schott North America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott Glass 8652 Sealing Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tungsten sealing glass, lower sealing temperature than glass 8651 Power diodesInformation provided by SCHOTT AG.
Physical Properties Metric English Comments
Density 3.18 g/cc

@Temperature 25.0 °C
0.115 lb/in³

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Modulus of Elasticity 58.0 GPa
8410 ksi
Poissons Ratio 0.25
0.25
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 - 300 °C
2.50 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Thermal Conductivity 0.900 W/m-K

@Temperature 90.0 °C
6.25 BTU-in/hr-ft²-°F

@Temperature 194 °F
Transformation Temperature, Tg 495 °C
923 °F
ISO 7884-8
Softening Point 638 °C
1180 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Working Point 900 °C
1650 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Annealing Point 490 °C
914 °F
Viscosity 10<sup>13</sup> dPa s; ISO 7884-4
Optical Properties Metric English Comments
Refractive Index 1.589

@Wavelength 587.6 nm
1.589

@Wavelength 587.6 nm
Electrical Properties Metric English Comments
Dielectric Constant 6.9

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
6.9

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
Dielectric Loss Index 0.0035

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
0.0035

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
Chemical Properties Metric English Comments
Acid Class, SR 4
4
DIN 12116
Alkali Class, AR 3
3
ISO 695
Descriptive Properties Value Comments
Hydrolytic Resistance Class HGB 1
ISO 719
Stress-optical Coefficient K (10-6mm2N-1) 3.4
DIN 52314
Users viewing this material also viewed the following: