Thermal Properties | Metric | English | Comments |
---|---|---|---|
Annealing Point | 490 °C | 914 °F | |
Ferro EG 3600 Metal Sealing Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Compress.Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched se.. |
|||
Annealing Point | 490 °C | 914 °F | |
Ferro F 2719 Metal Sealing Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Kovar Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals.. |
|||
Annealing Point | 490 °C | 914 °F | Viscosity 10<sup>13</sup> dPa s; ISO 7884-4 |
Schott Glass 8652 Sealing Glass Tungsten sealing glass, lower sealing temperature than glass 8651 Power diodesInformation provided by SCHOTT AG. |
|||
Annealing Point | 490 °C | 914 °F | |
Ferro EG 2964 Glaze and Sealant Glass Glass Type: Bi-Zn-B Typical Powder Form: VWG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and ins.. |