Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 495 °C | 923 °F | ISO 7884-8 |
Schott Glass 8652 Sealing Glass Tungsten sealing glass, lower sealing temperature than glass 8651 Power diodesInformation provided by SCHOTT AG. |