Polymer Property : Working Point = 1650 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Working Point 900 °C
1650 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Schott Glass 8652 Sealing Glass
Tungsten sealing glass, lower sealing temperature than glass 8651 Power diodesInformation provided by SCHOTT AG.