Physical Properties Metric English Comments
Density 2.69 g/cc
0.0972 lb/in³
Indium Corp. Indalloy 191 Aluminum Solder Alloy
Information Provided by Indium Corporation
Density 2.69 g/cc
0.0972 lb/in³
Schott BG42 Band Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Density 2.69 g/cc
0.0972 lb/in³
Constellium DOKIMA® Rolled Plate Aluminum
DOKIMA® rolled plates have moderate strength properties, a very low level of impurities, an excellent corrosion resistance, a very good dimensional stability and high thermal and electrical conduct..