Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.70 µm/m-°C @Temperature 20.0 - 300 °C |
4.83 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck WCu 80/20 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
CTE, linear | 8.70 µm/m-°C @Temperature 20.0 - 300 °C |
4.83 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott BG42 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 8.70 µm/m-°C @Temperature 20.0 - 300 °C |
4.83 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-BASF64 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.70 µm/m-°C @Temperature 20.0 - 1000 °C |
4.83 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec B 601 Alumina, 98.5% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
CTE, linear | 8.70 µm/m-°C @Temperature 20.0 - 1000 °C |
4.83 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec B 40 Alumina, 99.1% B 40 is the ideal sliding mate with the same properties as Rubalit® A 1896. It contains a larger share of Al2O3 for superior chemical stability. |
|||
CTE, linear | 8.70 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.83 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott BG28 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 8.70 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.83 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott BG25 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |