STAR Thermoplastic Alloys & Rubbers StarFlex® P 7130-1000 TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer STAR Thermoplastic Alloys & Rubbers
Trade Name StarFlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF STAR Thermoplastic Alloys & Rubbers StarFlex® P 7130-1000 TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: StarFlex P 7130-1000 is an easy processing TPE designed for injection molding. Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades availableProcessing Method: Injection MoldingInformation Provided by STAR Thermoplastic Elastomers
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Viscosity 6700 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
6700 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 30

@Time 10.0 sec
30

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 3.82 MPa

@Time 7200 sec
554 psi

@Time 2.00 hour
Die C; ASTM D414
Elongation at Break 977 %

@Time 7200 sec
977 %

@Time 2.00 hour
Die C; ASTM D412
300% Modulus 0.000503 GPa

@Time 7200 sec
0.0730 ksi

@Time 2.00 hour
Die C; ASTM D412
Tear Strength 8.77 kN/m
50.0 pli
ASTM D624
Descriptive Properties Value Comments